Rieter

Disentangling neps

Index

While the number of neps increases from machine to machine in the  blowroom, the card reduces the remaining number to a small fraction. It is often falsely assumed that neps are eliminated at the card; in fact, they are mostly opened out. Only a fraction of the neps leaves the machine unopened via the flat strippings. Fig. 87 shows the approximate change in the number of neps in the process.

An improvement in the disentangling of neps is obtained by:

  • reducing fiber density on the cylinder by using larger cylinder widths;
  • closer spacing between the clothing surfaces;
  • sharper clothing;
  • optimal (not too low) licker-in speeds;
  • low doffer speeds;
  • lower throughput.

Fig. 87 – Change in the number of neps in the cotton when passing blowroom and cards